Premix Premi-Glas® 1200H-24 Polyester SMC

 

Subcategory: Composite SMC; Polyester, TS; Thermoset

Key Words: Sheet Molding Compound

Material Notes:
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recognition properties is sufficient. Key features and benefits are:

  • Underwriters Laboratory listed for UL 94HB flame recognition at 1.47mm minimum wall thickness.
  • U.L flame recognized in all colors.
  • Excellent flexural strength and flexural modulus properties.
  • Designed for compression molding in matched metal molds.
  • Available in fiberglass content of 10-30%.
  • The Premi-Glas 1200-H series carries U.L 746 C recognition for use in exterior applications following ultraviolet light, water emersion and exposure testing.

Data provided by Premix.

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Yield Strength
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Dielectric Strength
  • Arc Resistance
  • Deflection Temperature at 1.8 MPa (264 psi)
  • UL RTI, Electrical
  • UL RTI, Mechanical with Impact
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。