Premix Premi-Glas® 8101-11C Polyester BMC

 

Subcategory: Polyester, TS; Thermoset

Material Notes:
Premi-Glas® 8101-11C is a 11percent glass reinforced thermoset, bulk molding compound designed for injection molded automotive forward lighting applications. Key features and benefits are:

  • Exhibits excellent dimensional stability and heat resistance.
  • Outstanding thermal stability permits smaller, low profile reflector designs.
  • Designed for high speed, automated injection processes.
  • Compatible with UV-curable base coats which are required for vacuum metallization.
  • Available in fiberglass reinforcement from 10-22 percent. Standard reinforcement content is 11 percent.
  • Processes in cold manifolds and hot sprue molds.
  • Molds on conventional screw and plunger injection machines.
  • Approved to GM 7001M UP, MG 2600.
  • Standard colors are gray and black.

Data provided by Premix.

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Tensile Strength, Ultimate
  • Flexural Modulus
  • Flexural Yield Strength
  • Deflection Temperature at 1.8 MPa (264 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。