Raschig Group Synres-Almoco B.V. SURAPLAST UPA 63

 

Subcategory: Thermoset; Polymer

Material Notes:
Short glass fiber reinforced, inorganically filled UP molding compound in grey (RAL 7035) and dark colors. Very low mould shrinkage and post-shrinkage, very high arc resistance, very high mechanical values, better than UP 804. Self-extinguishing (V-0/0,75 according to UL 94), UL-listed in colors grey and black. Free of halogens and toxic heavy metals. Forms: Low dust granulate, packed in moisture resistant bags. Standard bag size: 25 kg palletized in 1.000 kg loads or big-bags. Processing: Injection. Applications: Molded parts in electrical engineering with high heat resistance and high mechanical strength i.e.- Contact terminals, Relays, Automatic cut-outs (FI/LS).

Information provided by the Raschig Group

Available Properties
  • Specific Gravity
  • Apparent Bulk Density
  • Linear Mold Shrinkage
  • Ball Indentation Hardness
  • Tensile Strength, Yield
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • Comparative Tracking Index
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Deflection Temperature at 8.0 MPa
  • Flammability, UL94
  • Shrinkage
  • Front Barrel Temperature
  • Melt Temperature
  • Mold Temperature
  • Glow Resistance, class-mm
  • Glow-wire test, 960°
  • Needle-flame test
  • Water Absorption, max [mg]
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。