ChemRex® CX-26 Isocyanate-Free Polyurethane-Based Sealant

 

Subcategory: Adhesive; Polyurethane, TS; Thermoset

Key Words: ChemRex, Inc.

Material Notes:
CX-26 is a polyurethane based one-component, moisture curing sealant. It provides fast cure, non-sag, excellent adhesion and has elastomeric properties with high strength which can reduce/eliminate mechanical fasteners.

Typical applications of CX-26 include sealing of interior/exterior joints, waterproofing overlap seams, bonding or sealing side post, and sealing compartment doors.

Tack-free time is 17 minutes ± 2 minutes given the ASTM C 679 test method. Sag resistance is excellent given the ASTM C 639 test method. The tear strength is 32 pits ± 5 pits given the ASTM D 1044 test method. Adhesion-in peel is 39 pli ± 5 pli given the ASTM C 794 test method. The mandrel bend showed no cracking given the ASTM C 793 test method. Bond durability on glass, aluminum, and concrete is 12.5 % given the ASTM C 719 test method.

Information provided by ChemRex, Inc.

Available Properties
  • Density
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • Tear Strength Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。