Rhodia Technyl® A246M Nylon 66, Impact Grade, EH50

 

Subcategory: Nylon; Thermoplastic; Nylon 66

Key Words: Polyamide 66; PA66

Material Notes:
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.

Technyl A 246m offers an excellent notched impact resistance at low temperatures making it suitable for sports and leisure applications. It is suitable for shoe soles, ski components, ski and surf bindings, as well as toy applications, such as the bumper of a remote-controlled car.

This product is available in natural, white and black.

Information provided by Rhodia.

Available Properties
  • Density
  • Water Absorption
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Izod Impact Resistance
  • Electrical Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Comparative Tracking Index
  • Melting Point
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Moisture Content
  • Back Pressure
  • Fill Speed
  • Injection Speed (cm3/sec)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。