Rogers Bisco™ HT-840 Cellular Silicone Foam

 

Subcategory: Silicone; Elastomer, TS; Thermoset

Material Notes:
Extra firm grade silicone sponge. UL recognized of flame retardance.

Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination on skis and T-shirts

No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568 corrosion resistance. Passes SMP-800-C & BSS toxic gas emission rating. Passes hot flex at 230°C (446°F) per ASTM D-573.

General BISCO™ silicone information: BISCO™ Cellular Silicones are used as sealing cushioning, vibration isolation, insulation, and thermal management gaskets. Their resistance to environmental extremes, mechanical resilience, and safety features lead to their use in transportation equipment, communications and electrical enclosures, electronic products and components, industrial machinery, and appliances.

Data provided by Rogers Corporation.

Available Properties
  • Density
  • Water Absorption
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Compressive Yield Strength
  • Compression Set, Elevated Temperature
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Arc Resistance
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Brittleness Temperature
  • Flammability, UL94
  • Flame Spread Index
  • Smoke Density
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。