SHAMROCK NanoFLON® P 47A Thermoplastic Grade PTFE Additive

 

Subcategory: Additive/Filler for Polymer; PTFE

Material Notes:
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micron range (200 - 700 nanometers), as well as tightly-controlled chemical and physical properties. This significantly impacts molecular weight, crystallinity and morphology f the nanosized PTFE, thereby achieving key PTFE properties, including slip, refractive index, wettability surfactant and dielectric constant. NanoFlon P powder is agglomerated to 10 - 15 microns to minimize dusting during handling and is designed to disperse with regular mixing. the agglomerates break down with a resulting average particle size ranging from 200 - 700 nanometers. This provides up to one hundred times the surface area of other PTFE particles at equal weight (3µ vs. .3µ) for enhanced surface energy properties.

Application:High intensity dispersion recommended, such as Medium mill or twin screw extruder process

  • Offset, gravure and flexographic inks
  • Digital and electronic inks
  • Coatings: Industrial, automotive top coats, etc.
  • Optical coatings
  • UV protection
  • Fade resistance
  • Thermoplastic fibers
  • Plastic/Thermoplastic gears components
  • Wire and cable
  • Elastomeric seals and parts
  • Cosmetics, personal care products, hair care products and sunscreens
  • Lubricants, greases and oils
  • Agricultural chamicals and pesticides
  • Textile fibers
  • Electronics/Electrical coatings and componenets
  • Polymeric computer chips
Speciality: Smallest MV

Information provided by Shamrock Technologies

Available Properties
  • Particle Size
  • Melting Point
  • Appearance
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。