Dyna-Purge® SF Purging Compound

 

Subcategory: Purging Compound

Material Notes:
Designed for Sheet & Profile Co-Extrusion & Multi-Layer Film

General Description:

DYNA-PURGE SF is a non-abrasive, non-chemical “engineered” thermoplastic purging compound, with a proprietary foaming agent, which allows the purge to expand and scrub the screw and barrel, die, and other downstream equipment. The material is designed for extruders and co-extruders that have limited clearances related to screenpacks, mixing or metering devices, etc., when processing sheet, profile, and single or multi-layer blown film.

FEATURES & BENEFITS OF DYNA-PURGE SF

  • Excellent for color changes, resin changes, preventative machine maintenance, and before manual cleaning
  • Ideal for use when screen packs can’t be removed from the extruder, when the die head has clearance of less than .025 inch (.65 mm), or for when there are metering and mixing devices
  • Effective through a wide temperature range 320°F-575°F(160°C-302°C)
  • Easy to use – no process adjustment necessary – use at the resident resin processing temperature and RPM speed
  • Non-abrasive thermoplastic, which thoroughly loosens carbonized and degraded resin, allowing it to be flushed out of the system
  • Safe, non-hazardous, with no chemicals – ingredients are FDA compliant
  • Heat stable – recommended during shutdown and start-up
  • Low “cost-per-purge” – only small quantity needed to be effective
  • No mixing required – simply use “as is”
  • Unlimited shelf life
Dyna-Purge is the top performing purging compound on the market today. The product line offers superior cleaning and economic value over in-house methods and other commercial purging compounds. We invite you to sample Dyna-Purge at no charge, so you can prove it to yourself. Dyna-Purge, the industry leader for over 20 years!

Available Properties
  • Processing Temperature
  • Amount of Purge (Extrusion)
  • Screen Packs or other flow restrictions (Ext.)
  • Types of Resins
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。