SKYGREEN® PETG 2008, Specially Formulated PET Copolymer Resin

 

Subcategory: Polyethylene; Polyethylene Terephthalate (PET); Thermoplastic

Material Notes:
Description: SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processability and clarity. Skygreen® PETG provides a material having outstanding toughness, clarity, color, chemical resistance, and resistance to stress whitening. It can readily be thermoformed for extrusion blow molded. It is superior to acrylic for toughness, and superior to polycarbonate for processability.

Applications: Extrusion Sheet: architecture protective cover, display signs, industrial products. Extrusion Film: blister packaging, food packaging containers, electrical & electronic packaging, pharmaceutical & medical packaging. Injection Molding: toys, refrigerator parts, electric & electronic parts, smart cards, pen caps, medical devices and tools. Extrusion Blow Molding: bottles for cosmetics, soaps, shampoos, detergents, etc.

Information provided by SK Chemicals.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Linear Mold Shrinkage
  • Hardness, Rockwell R
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Impact Test
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Glass Temperature
  • Flammability, UL94
  • Processing Temperature
  • Feed Temperature
  • Nozzle Temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Adapter Temperature
  • Die Temperature
  • Head Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  • Injection Pressure
  • Hold Pressure
  • Back Pressure
  • Cycle Time - Injection
  • Cycle Time - Cooling
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。