HiMod® 914 Thermoplastic Bearing

 

Subcategory: Thermoplastic

Key Words: Busak + Shamban; TI Group; Smiths Group

Material Notes:
Thermoplastic Bearing

Characteristics: HiMod® 914 is a self lubricating bearing material developed for the most severe and critical applications. A high LPV along with superb chemical resistance, low moisture absorption, high modulus and low friction and wear rate, allow the solid of wear and friction problems in applications where only Polyamides similar to Vespel® were previously used. HiMod® 914 is an injection moldable engineered thermoplastic which gives the user considerable design freedom along with an economical form of manufacture.

Applications: Automotive under-hood components, industrial equipment, oil-field parts, photo processing components, exercise equipment, aircraft, forest industry

Information provided by Busak + Shamban, now a subsidiary of Smiths Group.

Available Properties
  • Limiting Pressure Velocity
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。