HiMod® 924 Thermoplastic Bearing

 

Subcategory: Thermoplastic

Key Words: Busak + Shamban; TI Group; Smiths Group

Material Notes:
Thermoplastic Bearing

Characteristics: HiMod® 924 is a high temperature, high modulus material developed for those functions that require high strength and high compressive properties along with excellent chemical resistance and low thermal expansion. This compound is known for its high flexural modulus, high compressive strength, low thermal expansion, superb chemical resistance, and low moisture absorption. It is also injection moldable.

Applications: Valve seats, gas turbine engine and automotive under-hood components, sliding vanes, aerospace, and medical

Information provided by Busak + Shamban, now a subsidiary of Smiths Group.

Available Properties
  • Moisture Absorption at Equilibrium
  • Flexural Modulus
  • Compressive Yield Strength
  • CTE, linear 20°C
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。