Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer

 

Subcategory: Ethylene Vinyl Alcohol; Thermoplastic

Key Words: EVOH

Material Notes:
High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.

The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a thin gas barrier layer without loss of shelf life.

Soarnol AT4403 with low melt flow index is one of the standard grade of Soarnol, its ethylene content is 44 mol%. Soarnol AT4403 has excellent water resistance and has a gas barrier property that does not drastically lower at high humidity, so Soarnol AT4403 can be used as the most outer layer of multi layer film. This resin suited for coextruded inflation film and coextruded sheet.

Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.

Available Properties
  • Density
  • Moisture Vapor Transmission
  • Oxygen Transmission
  • Viscosity
  • Melt Flow
  • Melting Point
  • Crystallization Temperature
  • Glass Temperature
  • Refractive Index
  • Haze
  • Nozzle Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。