Solvay Advanced Polymers KetaSpire™ KT-820 GF30 Polyetheretherketone, 30% Glass Reinforced

 

Subcategory: Polyetheretherketone (PEEK); Thermoplastic; Polymer

Material Notes:
KetaSpire KT-820 GF30 is the low-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire PEEK resin. Reinforcement also affords greater mechanical robustness in structural applications, particularly those with service temperatures approaching 300°C.

KetaSpire PEEK is produced to the highest industry standards and is characterized by a distinct combination of best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids, and bases.

These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing, and other industrial uses. KetaSpire KT-820 GF30 can be easily processed using typical injection molding and extrusion processes.

Information provided by Solvay Advanced Polymers

Available Properties
  • Specific Gravity
  • Water Absorption
  • Melt Flow
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • CTE, linear 20°C
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。