Solvay Advanced Polymers PrimoSpire™ PR-250 Self-Reinforced Polyphenylene

 

Subcategory: Thermoplastic

Material Notes:
PrimoSpire self-reinforced polyphenylenes (SRPs), formerly marketed as Parmax, are ultra-high performance amorphous, melt-processable engineering thermoplastics. The unique properties of these materials are due primarily to the inherent rigid-rod structure. PrimoSpire SRPs are differentiated from other thermoplastics by outstanding mechanical properties without fiber reinforcement, scratch resistance, excellent solvent resistance, and exceptional low temperature performance.

In addition, PrimoSpire SRP has great thermal and thermal-oxidative stability, is noncombustible, presents higher specific strengths than many of the materials commonly encountered in structural applications, and also possesses excellent machinability. The outstanding mechanical, chemical, thermal, and physical properties of PrimoSpire SRP make it the material of choice for a variety of applications including aircraft substructures, semiconductor components, gears, light-weight vehicle suspensions systems, medical tubing and other medical devices.

PrimoSpire PR-250 resin is a developmental injection molding grade of ultra-high performance engineering thermoplastic. It is similar to our PrimoSpire PR-120 resin but with lower viscosity and consequently better flow performance at high temperatures making it especially well-suited for parts requiring injection molding capabilities. PrimoSpire PR-250 resin is commercially available in natural or black pellets for extrusion, compression or injection molding, or in a powder form.

Information provided by Solvay Advanced Polymers

Available Properties
  • Specific Gravity
  • Water Absorption
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。