Solvay Engineered Polymers NEXPRENE® 1155A TPV - FDA Grade

 

Subcategory: Elastomer, TPE; Polypropylene; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes:
Description: NEXPRENE® 1155A thermoplastic vulcanizate (TPVs) is a fully cross-linked EPDM/PP compound designed to replace thermoset elastomers, such as polycholorpene (Neoprene) or EPDM, and conventional thermoplastic rubber. NEXPRENE® 1155A complies with FDA, CFR title 21-Section 177.2600 and CFR title 21 Section 177.1210. NEXPRENE rubber provides the advantage of low cost thermoplastic processing, such as injection molding, extrusion, and blowmolding.

Applications: Rubber articles intended for repeated use in contact with non-fatty and non-oily foods are covered under section 177.2600. Section 177.1210 also covers rubber articles deemed safe for single-use closure and sealing gaskets in contact with non-fatty and non-oily foods. NEXPRENE® 1100 grades are suitable for FDA components such as valves, gaskets, peristaltic pump tubes, diaphragms, tubing, seals, and cable jacketing.

Information provided by Solvay Engineered Polymers.

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • Tear Strength
  • Compression Set
  • Brittleness Temperature
  • Oil Resistance IRM 903
  • Ozone Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。