Solvay Advanced Polymers Acudel™ 22000 Polyphenylsulfone Blend

 

Subcategory: Polyphenylsulfone; Thermoplastic

Close Analogs:

Information provided by Solvay Advanced Polymers.

Material Notes:
ACUDEL 22000 is a polyphenylsulfone-based polymer blend. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases, and good resistance to stress cracking under a broad range of chemical environments. In addition to these attributes, ACUDEL 22000 resin exhibits robust toughness and improved notch resistance compared to both UDEL® polysulfone and RADEL® A polyethersulfone, although slightly lower than that of neat RADEL® R polyphenylsulfone. In general, the performance profile of ACUDEL 22000 resin is intermediate between that of polysulfone and polyphenylsulfone.

In addition to its high mechanical and thermal performance attributes, ACUDEL 22000 resin also offers very good electrical properties over a broad temperature range as well as inherent flame retardancy. The material exhibits excellent flow characteristics and can be readily processed using conventional injection molding equipment.

The “natural” version of ACUDEL 22000 is designated ACUDEL 22000 NT15 and its color is an opaque light beige. It is available in black as ACUDEL 22000 BK937 resin. ACUDEL 22000 resin can also be made available in a variety of colors.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Water Absorption at Saturation
  • Linear Mold Shrinkage
  • Melt Flow
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Tensile Impact Strength
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。