Saint-Gobain Norton® PMP Film

 

Subcategory: Polymethylpentene; Thermoplastic; Polymer

Material Notes:
Features/Benefits:

  • Good release properties for up to 180°C (356°F) cure composites (application dependent)
  • low density for high surface area per pound
  • Excellent clarity
  • Thermoformable
  • Product available in standard widths up to 60"
  • Product available with a minimum thickness of 0.0012" (30µm)
  • Clear or blue films
Low Density, High Yield Polymethylpentene Film
Norton® PMP film is manufactured from polymethylpentene (PMP) copolymer resin. This product offers high temperature resistance, superior optical characteristics, and lowest density among all polymer materials to deliver superior performance at a value price point.

Optical/Lamination Applications
Norton® PMP is manufactured with a gloss finish without plasticizers, stabilizers, or other processing aids, offering a clean surface for laminate manufacturing. Medical device manufacturers receive a high-clarity product well suited for optical measurement requirements. The non-stabilized polymer provides integrity for tested samples and a high surface coverage due to the low density.

Composite Fabrication
Norton® PMP offers manufacturers of composite products a material which will perform up to 180°C (356°F), depending on the specific application, for autoclave constructions. Applications such as golf shaft manufacture, aircraft lavatory components, and printed circuit boards benefit from the high surface area yield (due to the low density of this polymer), offering productivity savings for a single use product. Flexible printed circuit constructions utilize the release characteristics of Norton® PMP to provide protection from flowing adhesives during lamination processes.

Rubber Manufacturing
Norton® PMP film is an excellent candidate for applications involving the curing of rubber films and sheets. The excellent release characteristics and the non-plasticized formulation are advantageous for curing silicone rubber where coated PET may be unacceptable. Surface Treatment Available: Corona Treatment (1 or 2 sides)
Used for Aerospace/Release Films, Electrical/Electronics
Information provided by Saint Gobain Performance Products.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear 68°F
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Vicat Softening Point
  • Flammability, UL94
  • Oxygen Index
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。