    Saint-Gobain Norton® PVDF Fluoropolymer Film

     

    Subcategory: Fluoropolymer; Thermoplastic; PVDF; Polymer

    Material Notes:
    Features/Benefits:

    • Excellent weatherability
    • High dielectric strength
    • Excellent chemical and abrasion resistance
    • Thermoformable
    • Product available in widths up to 60"
    • Product available with thicknesses from 0.001" (0.0254 mm) to 0.020" (0.5 mm)
    • Temperature range of -62°C (-80°F) to 150°C (300°F)
    Weatherable, Chemically Resistant Fluoropolymer Film
    Norton® PVDF film is manufactured from polyvinylidene fluoride resin. This product offers the best weathering characteristics of any fluoropolymer film available. Norton® PVDF provides very good performance when subjected to severe conditions such as heat fluctuation, UV exposure, and corrosive environments. Norton® PVDF is manufactured to strict standards for gels and gauge control, offering the best value for fluoropolymer performance of any film. This material also performas over a wide temperature range, from -62°C (-80°F) to 150°C (300°F).

    Chemical Protection
    Norton® PVDF film protects against exposure to many common acids, oxidizing agents, and organics. This broad range of chemical resistance makes Norton® PVDF an excellent candidate for pump diaphragms and tank linings. The thin gauge films offer bondability for protection of equipment exposed to air pollutants, corrosive media, and weather.

    Decorative Applications
    Norton® PVDF film can be adaptable to metallizing or printing for a variety of protective applications. The excellent chemical resistance to a wide tange of cleaners and harsh cleaning agents used in high traffic applications offers long maintenance performance. Norton® PVDF carries a UL V-0 flammability rating, which signifies self-extinguishing performance suited for aircraft interior panel applications.

    Weathering Applications
    The outstanding weatherability of Norton® PVDF film makes it an excellent candidate for products with outdoor exposures. Vinyl siding is protected with excellent chemical and abrasion resistance of Norton® PVDF film. The fluoropolymer properties are impervious to UV expsure and eliminate wear due to water and chemical exposures. PVDF = polyvinylidene fluoride
    Used for Chemical Process, Electrical/Electronics, Protective/Decorative.
    Information provided by Saint Gobain Performance Products.

    Available Properties
    • Specific Gravity
    • Water Absorption
    • Tensile Strength, Yield
    • Elongation at Break
    • Tensile Modulus
    • Surface Resistivity per Square
    • Dielectric Constant
    • Dielectric Strength
    • Dissipation Factor
    • CTE, linear 68°F
    • Specific Heat Capacity
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Flammability, UL94
    • Oxygen Index
    • Refractive Index
    • Fold Endurance (MIN)
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。