Saint-Gobain Rulon® ACM Grade Bearing/Seal PTFE

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE; Polymer;

Material Notes:
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion. PTFE = polytetrafluoroethylene

ACM Grade Bearing/Seal PTFE: Laminates composed of synthetic fabrics impregnated by thermosetting resins and solid lubricant fillers. Material available in tubes and sheets. Ideally suited for non-lubricated ultra high-load/low-speed applications that require a low coefficient of friction. Operates well in demanding and destructive environments. Material does not have thermal and electrical insulating properties. Suitable for use in steam, wet, dry, or vacuum environments. Rc 35 or higher steel mating surface. Markets for ACM grade include Agricultural, Appliances, Automotive, Construction, Industrial, Transportation.
Information provided by Saint Gobain Performance Products.

Available Properties
  • Compressive Yield Strength
  • Machinability (1-10; 1 = easiest)
  • Dimensional Stability (1-4; 4 = highest)
  • Limiting Pressure Velocity
  • Others
  • Acetaldehyde Aq. (40%)
  • Acetamide Aq. (50%)
  • Acetic Acid Aq. (10%)
  • Acetone
  • Acrylonitrile
  • Alcohols, Aliphatic
  • Allyl Alcohol
  • Allyl Chloride
  • Aluminum Chloride Aq. (10%)
  • Aluminum Sulfate Aq. (10%)
  • Ammonia Aq. (10%)
  • Ammonia Gas
  • Ammonium Carbonate Aq. (10%)
  • Ammonium Chloride Aq. (10%)
  • Ammonium Chloride Aq. (37%)
  • Amyl Acetate
  • Amyl Alcohol
  • Aniline
  • Antimony Trichloride Aq. (10%)
  • Barium Chloride Aq. (10%)
  • Barium Sulfate Aq. (10%)
  • Barium Sulfide Aq. (10%)
  • Benzaldehyde
  • Benzene
  • Benzenesulfonic Acid
  • Benzoic Acid Aq. (SAT)
  • Benzyl Alcohol
  • Beverages Aq. Alcoholic
  • Beverages Aq. Carbonated
  • Bitumen
  • Bleaching Lye (10%)
  • Boric Acid Aq. (10%)
  • Boron Trifluoride
  • Bromine Aq. (30%)
  • Bromine Liq.
  • Butanol
  • Butyl Acetate
  • Butyl Phthalate
  • Butylene Glycol
  • Butyric Acid (CONC)
  • Butyric Acid Aq. (20%)
  • Calcium Chloride Aq. (10%)
  • Calcium Hypochlorite
  • Camphor
  • Carbon Disulphide
  • Carbon Tetrachloride
  • Carbonic Acid Aq. (10%)
  • Castor Oil
  • Chloral Hydrate
  • Chlorine Aq. (10%)
  • Chlorine Gas (100%)
  • Chloroacetic Acid Aq. (10%)
  • Chlorobenzene
  • Chloroform
  • Chlorosulfonic Acid Aq. (10%)
  • Chrome Alum Aq. (10%)
  • Chromic Acid Aq. (1%)
  • Citric Acid Aq. (10%)
  • Citric Acid Aq. (SAT)
  • Coconut Oil
  • Creosote
  • Cresols
  • Cresylic Acid
  • Cupric Chloride Aq. (10%)
  • Cupric Sulfate Aq. (0.5%)
  • Cupric Sulfate Aq. (10%)
  • Cupric Sulfate Aq. (SAT)
  • Cyclohexane
  • Cyclohexanol
  • Cyclohexanone
  • Detergents, Organic
  • Dibutylphthalate
  • Dichlorodifluoro Methane
  • Dichloroethylene
  • Diesel Oil
  • Diethyleneglycol Aq. (90%)
  • Dimethyl Aniline
  • Dimethyl Carbinol
  • Dimethyl Formamide
  • Dioxane
  • Edible Oils
  • Ethanol, Denatured (96%)
  • Ether, Diethyl
  • Ethyl Acetate
  • Ethyl Butyrate
  • Ethyl Chloride
  • Ethylene Chloride
  • Ethylene Chlorohydrin
  • Ethylene Diamine
  • Ethylene Dichloride
  • Ethylene Glycol Aq. (96%)
  • Ferric Chloride Aq. (10%)
  • Ferric Chloride Aq. (5%)
  • Ferric Chloride Aq. (SAT)
  • Ferrous Chloride Aq. (10%)
  • Fluorine (Gas Wet)
  • Fluorosilicic Acid Aq.
  • Formaldehyde Aq. (10%)
  • Formic Acid Aq. (10%)
  • Formic Acid Aq. (3%)
  • Freon 12 (Arcton 12)
  • Fruit Juices (CONC)
  • Furfural
  • Gasoline
  • Glycerine
  • Heptane
  • Hexane
  • Hydrobromic Acid Aq. (10%)
  • Hydrochloric Acid Aq. (0.4%)
  • Hydrochloric Acid Aq. (10%)
  • Hydrochloric Acid Aq. (2%)
  • Hydrofluoric Acid Aq. (4%)
  • Hydrogen Peroxide Aq. (0.5%)
  • Hydrogen Peroxide Aq. (1%)
  • Hydrogen Peroxide Aq. (3%)
  • Hydrogen Sulfide Aq. (SAT)
  • Hydrogenated Vegetable Oils
  • Hydroquinone
  • Iodine (3%)
  • Iodine (in Alcohol)
  • Iso octane
  • Isopropyl alcohol
  • Isopropyl Ether
  • Lactic Acid Aq. (10%)
  • Lactic Acid Aq. (90%)
  • Lead Acetate Aq. (10%)
  • Linseed Oil
  • Lithium Bromide Aq. (50%)
  • Lubricating Oils (Petroleum)
  • Magnesium Chloride Aq. (10%)
  • Magnesium Hydroxide Aq. (10%)
  • Magnesium Sulfide Aq. (10%)
  • Maleic Acid Aq. (CONC)
  • Malonic Acid Aq. (CONC)
  • Manganese Sulfate Aq. (10%)
  • Mercuric Chloride Aq. (6%)
  • Mercury
  • Methanol
  • Methy Phenyl Ether
  • Methyl Acetate
  • Methyl Ethyl Ketone
  • Methylene Chloride
  • Methylpyrrolidone
  • Milk
  • Mineral Oils
  • Naphthalene
  • Nickel Sulfate Aq. (10%)
  • Nicotine
  • Nitric Acid Aq. (0.1%)
  • Nitric Acid Aq. (10%)
  • Nitrobenzene
  • Nitromethane
  • Oleic Acid
  • Oxalic Acid Aq. (10%)
  • Ozone
  • Paraffin
  • Perchloric Acid Aq. (10%)
  • Perchloroethylene
  • Petroleum Ether
  • Phenol Aq. (6%)
  • Phenol Aq. (75%)
  • Phosphoric Acid Aq (0.3%)
  • Phosphoric Acid Aq (3%)
  • Phosphoric Acid Aq. (10%)
  • Phthalic Acid Aq. (SAT)
  • Potassium Acetate Aq. (50%)
  • Potassium Bicarbonate Aq. (60%)
  • Potassium Bromide Aq. (10%)
  • Potassium Carbonate Aq. (60%)
  • Potassium Chloride Aq. (90%)
  • Potassium Dichromate Aq. (5%)
  • Potassium Ferricyanide Aq. (30%)
  • Potassium Ferrocyanide Aq. (30%)
  • Potassium Hydroxide Aq. (10%)
  • Potassium Hydroxide Aq. (50%)
  • Potassium Nitrate Aq. (10%)
  • Potassium Permanganate Aq. (1%)
  • Potassium Sulfite Aq. (90%)
  • Potassium Sulfite Aq. (CONC)
  • Propane Gas
  • Pyridine
  • Resorcinol
  • Salicylic Acid
  • Silicone Fluids
  • Silver Nitrate
  • Soap Solutions
  • Sodium (Molten)
  • Sodium Acetate Aq. (60%)
  • Sodium Benzoate Aq. (10%)
  • Sodium Bicarbonate Aq. (50%)
  • Sodium Bisulphite Aq. (10%)
  • Sodium Bromide Aq. (10%)
  • Sodium Carbonate Aq. (20%)
  • Sodium Carbonate Aq. (50%)
  • Sodium Chlorate Aq. (10%)
  • Sodium Chloride Aq. (10%)
  • Sodium Chloride Aq. (90%)
  • Sodium Cyanide Aq. (10%)
  • Sodium Hydroxide Aq. (10%)
  • Sodium Hydroxide Aq. (50%)
  • Sodium Hypochlorite 15% CI (Chlorine Bleach)
  • Sodium Nitrate Aq. (50%)
  • Sodium Perborate Aq. (10%)
  • Sodium Phosphates Aq. (General)
  • Sodium Silicate
  • Sodium Sulfate Aq. (90%)
  • Sodium Sulfide Aq. (90%)
  • Sodium Thiosulfate Aq. (10%)
  • Stannic Chloride Aq. (10%)
  • Stannic Sulfate Aq. (10%)
  • Stearic Acid
  • Styrene (Monomer)
  • Sulfur
  • Sulfur Dioxide (Dry Gas) (100%)
  • Sulfuric Acid Aq. (2%)
  • Sulfuric Acid Aq. (5%)
  • Sulfuric Acid Conc.
  • Sulfurous Acid Aq. (10%)
  • Tallow
  • Tar
  • Tartaric Acid Aq.
  • Tetrachlorethylene
  • Tetrahydrofuran
  • Thionyl Chloride
  • Thiophene
  • Toluene
  • Transformer Oil
  • Trichlorethylene
  • Triethanolamine
  • Trisodium Phosphate Aq. (95%)
  • Turpentine
  • Urea
  • Vaseline
  • Vegetable Oils
  • Vinegar
  • Vinyl Chloride
  • Water
  • Wax (Molten)
  • White Spirit
  • Wines & Spirits
  • Xylene
  • Xylenol
  • Zinc Chloride Aq. (10%)
  • Zinc Oxide
  • Zinc Sulfate Aq. (10%)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。