Saint-Gobain Norton® Tygon® Inert Tubing Formulation SE-200

 

Subcategory: Thermoplastic

Material Notes:
Description: Tygon® SE-200: Without sacrificing the flexibility, glass-like clarity or outstanding bend radius for which Tygon® tubing is known, Tygon® Inert Tubing can handle many applications where flexible tubing of the past could not be used. Its FEP inner liner provides the ultimate in chemical resistance and can handle a wide variety of fluids from corrosives to MEK-based solvents. The liner is inert, meaning it will not extract or contaminate fluids being transferred. The fluid path will not impart odor or taste, making it well-suited for food and beverage use. It meets FDA criteria for food and beverage applications, as well as USP Class VI criteria for biocompatibility. Tygon® Inert Tubing combines all the benefits of Tygon® with the inertness of a fluoropolymer, providing superior performance in many applications and industries.

Features/Benefits:

  • Crystal Clarity
  • Improved flexibility when compared to rigid fluoropolymer tubings
  • Chemically resistant and inert
  • Non-contaminating fluid path
  • Meets FDA and USP Class VI Criteria
Typical applications include Chemical Processing, Pharmaceutical Processing and Filling, Paint and Solvent Production and Packaging, Adhesive Transfer Lines, Semiconductor Processing, Photographic Processing Equipment, Beverage Dispensing, Ink and Toner Feed Lines, Fertilizer and Pesticide Distribution.
Information provided by Saint Gobain Performance Products.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • 100% Modulus
  • 300% Modulus
  • Tear Strength
  • Compression Set, Elevated Temperature
  • Tensile Set
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Brittleness Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。