Saint-Gobain Norton® Tygon® Plasticizer Free Tubing Formulation 2001

 

Subcategory: Thermoplastic

Material Notes:
Description: Tygon® 2001: Tygon® Plasticizer Free Tubing is a uniquely engineered product that offers the low compression set properties of a thermoset rubber. Tygon® Plasticizer Free Tubing provides the most flexibility, highest temperature resistance and longest pump life available in a clear, plasticizer / oil free tubing. It is ideal for a broad range of applications including peristaltic pump applications, soap and detergent dispensing, water purification lines, food contact applications and chemical transfer. This uniquely engineered tubing will not embrittle or crack prematurely like other tubings that contain plasticizer or extender oils, benefiting the user with less downtime and tubing changes.

Features/Benefits:

  • Plasticizer and oil free -- does not contaminate fluids
  • Superior flex life in peristaltic pumps
  • Chemically resistant to a wide range of fluids
  • Temperature resistant from -108°F to 135°F
  • Clear for easy visual flow monitoring
  • Meets FDA criteria for food contact
Ideal for a broad range of demanding applications including peristaltic pump systems, soap and detergent dispensing, ink transfer, water purification lines, food and beverage, and chemical transfer.
Information provided by Saint Gobain Performance Products.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • 100% Modulus
  • Tear Strength
  • Compression Set, Elevated Temperature
  • Tensile Set
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Brittleness Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。