Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber

 

Subcategory: Silicone; Elastomer, TPE; Thermoplastic

Material Notes:
Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durometer to the relatively hard 70 durometer on the Shore A scale. It is manufactured in different formulations to provide a choice of physical properties and cost considerations. 9200 Series: COHRlastic 9200 High Performance Series provides excellent tensile strength and superior tear resistance. It is tougher and more resilient than general-purpose silicone. Standard thicknesses are 1/32", 1/16" and 1/8", and it withstands temperatures ranging from -100°F to +400°F. A minimum thickness of 0.015" is available on a minimum quantity basis. All data based on a 0.0625 inch test sample.(Also comes in thicknesses from 1/32" to 1/8")
Information provided by Saint Gobain Performance Products.

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • Tear Strength
  • Compression Set, Elevated Temperature
  • Dielectric Strength
  • CTE, linear 68°F
  • Specific Heat Capacity
  • Thermal Conductivity
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。