Saint-Gobain COHRlastic® F-12 Silicone Foam

 

Subcategory: Silicone; Thermoplastic

Material Notes:
Description: Low-density, flame-retardant COHRlastic silicone foam yard goods provide outstanding performance for industries ranging from aviation and mass transit to automotive, electronics, construction and furniture. In addition to a UL94V-O listing in thicknesses down to 1/16", it withstands a 2100°F flame for more than 10 minutes without burning through in thicknesses down to 3/8". The material, which has a nominal density of 12 pounds per cubic foot, generates very little white smoke. Non-corrosive for use with metals and in hostile environments, it has low compression set. Among its applications are fireblocks, thermal barriers, noie and vibration dampeners, insulationa dn high-performance gaskets or seals. For the aviation, automotive and mass transit industries, it offers a high degree of design flexibility. Lightweight and easy to process, it can be laminated to seat cover fabrics and carpeting as a backing for added flame resistance in passenger compartment furnishings. The material has similar uses in institutional and residential furnishings, marine and lighting applications. It offers properties valuable in flame retardant backings for floor, wall and furniture coverings; fire-wall and thermal barriers or insulation, padding and gasketing for commercial and private marine vehicles; or gasketing and sealing in high-intensity light fixtures and electronic components in medial, computer and business equipment. Supplied in 18" and 36" wide roll stock. Thicknesses are shown in the table below. It is available plain or, on special order, laminated to any of a wide range of substrates. Because of the unique nature of COHRlastic foam, SGPPL CHR has undertaken a rigorous testing program which is performed at outside independent laboratories. The tests document the flame resistant properties and low levels of toxicity and smoke generation as well as mechanical and electrical properties. Details are on file at SGPPL CHR.

  • Passes FDA Extractables, 21 CFR177.2600
  • Products Combustion (ASTM E662), Hydrogen Cyanide = 0 ppm
  • In compliance with Boston Fire Dept. Chair Test, January 1986
  • Passes FAR 25.853(a) and (b)
  • Passes UL94V-0
All data based on a 0.0625 inch test sample.(Other thicknesses available.)
Information provided by Saint Gobain Performance Products.

Available Properties
  • Density
  • Tensile Strength, Yield
  • Elongation at Break
  • Compressive Strength
  • Compression Set, Elevated Temperature
  • Insulation Resistance
  • Dielectric Constant
  • Arc Resistance
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Flame Spread Index
  • Smoke Density
  • Oxygen Index
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。