Saint-Gobain Norton® Norseal® V780 Medium-Density Pressure Sensitive Adhesive Sealant Foam

 

Subcategory: Adhesive; Thermoplastic

Material Notes:
Description: Improved Performance: Norseal® V780 medium density foam sealant combines a closed cell foam substrate with a one-sided pressure-sensitive adhesive. Norseal has been specially formulated to provide superior performance with a reduced density foam, and is ideal for applications such as small appliance seals, corrugated wall seals, machinery enclosures, buses and off-road vehicles, HVAC seals, and window and door seals.

Closed Cell Foam: Meets FMVSS 302 Flammability Standard; Superb closed cell structure of foam uses less material to achieve a positive seal; Consistent seal with a minimum of 30% compression; Available in black.

Pressure-Sensitive Adhesive: High performance adhesive coating eliminates messy adhesive application; Liner is on the non-adhesive side. The roll stays together during handling with no stretching when applied.

Medium Density: Specially formulated to provide high performance with a reduced density foam; Excellent weathering, oxidation and fungi resistance provides long life; Formulated to prevent water infiltration on irregular surfaces.

Features/Benefits: Multipurpose medium density closed cell foam uses less material to achieve a positive seal; Meets FMVSS 302 Flammability Standard; Prevents water infiltration on irregular surfaces; Resistant to weather, Fungi and Oxidation; Broad service temperature range; Dimensionally stable.

Typical applications include: Corrugated wall seals, lighting equipment, small appliances, door and window seals, machinery enclosures, buses and off-road vehicles, concrete forms, HVAC seals. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/16" to 3/8".)
Information provided by Saint Gobain Performance Products.

Available Properties
  • Density
  • Water Absorption
  • Hardness, Shore OO
  • Tensile Strength, Yield
  • Elongation at Break
  • Compressive Strength
  • Compressive Modulus
  • Compression Set
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。