Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam

 

Subcategory: Polyurethane, TP; Thermoplastic

Material Notes:
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microcellular foams are categorized by degree of deflection force. By varying the modulus and density, Saint Gobain Performance Plastics has developed this series of materials that meets the demands of design engineers today. All Korel fians are available with an aggressive acrylic adhesive on one side to facilitate placement. Korel K60 series is very firm, high-deflection urethane foam. This series offers very tight tolerance for gauge control. Its high internal strength resists tearing and deformation.

FEATURES/BENEFITS:

  • Excellent compression set resistance
  • Highly resilient (will not collapse)
  • Dissipates stresses
  • Resistant to moisture and most chemicals
  • Conformable and flexible even in extreme environmental conditions
  • Easy to achieve intricate die-cut parts
  • Aggressive acrylic adhesive (optional) facilitates assembly
  • Available cast on to polyester film for stability and low deformation
Typical Applications: Cellular telephones, electrical enclosures, electronic gasketing, vibration damping, cushioning, acoustical control, bumpers, instrument panels, spacers.
Specification Notes: UL Testing (JMST2) UL 50 and UL 508 File MH26338; Passes Fogging Test SAE-J 1756, 3 hrs. at 212°F (100°C). All data based on a 0.012 inch test sample.
Information provided by Saint Gobain Performance Products.

Available Properties
  • Density
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Compressive Modulus
  • Tear Strength
  • Compression Set
  • Compression Set, Elevated Temperature
  • Volume Resistivity
  • Surface Resistivity per Square
  • Dielectric Strength
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Standard Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。