Saint-Gobain Norton® Norseal® V760 High Density Vibration Dampening Foam Sealant

 

Subcategory: Vinyl; Thermoplastic

Material Notes:
Description: Seals and Dampens Vibration: Norseal® V760 is a closed-cell PVC foam sealant with a pressure-sensitive adhesive on one side. Its high-density structure and multitude of tiny cells act like shock absorbers to seal and dampen vibration. Firm, High Density Foam for Positive Seals: This shock-absorbing feature makes Norseal V760 ideal for die-cut applications and metal-to-metal sealing. Versatile and easy to use, Norseal V760 is designed to produce a positive seal in mechanically fastened assemblies with as little as 30 percent compression. Conformable and Dimensionally Stable: Norseal V760 provides excellent conformability to curved and irregular shapes. It is resistant to weather, fungi and oxidation, ensuring a long sealing life. In addition, Norseal V760 is dimensionally stable. It will not drip, ooze or run under compression, and remains flexible at low temperatures. Pressure Sensitive Adhesive: The aggressive pressure-sensitive adhesive on one side of Norseal V760 facilitates high-speed application. The easy-peel paper liner eliminates stretching during installation, and removes easily after application. Norseal V760 series is available in gray. For specific low energy plastics, a specially formulated adhesive, "LE" is available.

FEATURES/BENEFITS:

  • Dimensionally stable under compression
  • Good abrasion resistance
  • Design facilitates high-speed application
  • Liner removes easily after application
  • Resistant to wether, fungi and oxidation
  • Low water absorption for long sealing life
  • Provides insulating properties
Applications: Truck trailer joint seals, door frame assemblies, concrete forms, export container seals, die-cut gaskets, roof sealing for parapets, duct seals, appliance seals, truck cab overlap seals. All data based on a 0.125 inch test sample.(Available in multiple thicknesses.)
Information provided by Saint Gobain Performance Products.

Available Properties
  • Density
  • Water Absorption
  • Hardness, Shore OO
  • Tensile Strength, Yield
  • Elongation at Break
  • Compressive Strength
  • Compressive Modulus
  • Compression Set
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。