STRUKTOL® VLB 618 Processing Additive

 

Subcategory: Additive/Filler for Polymer

Material Notes:
Blend of fatty acid esters. STRUKTOL® VLB-618 is manufactured from high quality vegetable fatty acids.

Applications: STRUKTOL® VLB-618 is the vegetable version of VLB-602 and is a very compatible complex ester lubricant. It has noted performance in clear calendared PVC sheet. It also has application in clear extrusion, blow molding and injection molding formulations. It is especially useful in products that require printing, laminating, or bonding. STRUKTOL® VLB-618 is very effective mostly as an external lubricant, with some internal properties, which have no negative impact on clarity in extrusion, calendering, or injection molding. STRUKTOL® VLB-618 is noted to have ideal characteristics for calendared sheet where clarity and low water blush is critical and where lower cost in performance is needed to replace montanic esters.

Information provided by Struktol

Available Properties
  • Specific Gravity
  • Dropping Point
  • Shelf Life
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。