Zell-Metall Engineering Plastics ZELLAMID® 1400 (PET) at 50% RH

 

Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic

Material Notes:
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.

This PETP features outstanding dimensional stability, as it is virtually unaffected by ambient moisture. A low coefficient of friction and excellent wear resistance combined with low creep and high modulus make this the choice material for moving parts. Hot water resistance is low.

Zellamid® 1400 is produced without centerline porosity. This material exhibits properties which make it suited to particular applications, especially high precision components.

Typical applications are components for foodprocessing machines, mandrels, liquid and gas proof parts, electrical engineering and all parts where Acetal’s microporosity in the centerline is not desirable.

For friction applications we offer Zellamid® 1400T (PETP with a solid lubricant) which shows a significantly reduced friction coefficient and increased resistance to wear.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Dart Drop, Total Energy
  • Comparative Tracking Index
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • FMVSS - 302 flame propagation rate
  • Time yield limit
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。