Trichloroethylene (TCE; CHClCCl2)

 

Subcategory: Fluid

Close Analogs:

Information provided by Enviro Tech International and the reference(s).

Key Words: Trichloroethane, CHClCCl2

Material Notes:
Trichloroethylene is a colorless liquid which is used as a solvent for cleaning and degreasing metal parts. It is being phased out of many uses due to environmental and health concerns.

Available Properties
  • Density
  • Specific Gravity
  • Viscosity
  • Molecular Weight
  • Vapor Pressure
  • Surface Tension
  • Heat of Vaporization
  • Specific Heat Capacity
  • Melting Point
  • Boiling Point
  • Flammability Test
  • Atmospheric Lifetime
  • CAS Number
  • Evaporation Rate (n-Butyl Acetate = 1)
  • Flash Point TCC
  • Hansen Parameter Non-Polar
  • Hansen Parameter Polar
  • Hildebrand Parameter
  • Kauri Butanol Number
  • Ozone Depletion Potential (ODP)
  • Vapor Density (air = 1)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。