Blue River Coatings Low VOC Primer Sealer

 

Subcategory: Thermoset; Polymer

Material Notes:
BLUE RIVER COATINGS LOW VOC PRIMER SEALER is a high quality, single component primer. Performance obtained is equal or superior to that of single component solvent primers. LOW VOC PRIMER SEALER offers good coverage, excellent durability, and ease of application, as well as being a low VOC and EPA compliant coating.

Enviromental Advantages:BLUE RIVER COATINGS LOW VOC PRIMER SEALER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent exterior durability
  • Excellent hardness/impact resistance
  • Excellent mar and abrasion resistance
  • Excellent adhesion on plastics and gel coat substrates
  • Solvent resistant
  • Can be applied in a wide variety of temperature and humidity conditions without the use of retarders
  • Distilled water is used for reduction
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • Can be oven baked
  • Wide range of colors
  • Coating will not flash rust on bare metal
  • Shelf life of 1 year
  • Unused paint can be returned to container
  • Non-Flammable
  • Uses

  • Steel
  • Metal
  • Corrosion Resistance – ASTM B117, Good corrosion resistance – Pass at 450 hours. Coating was applied at 1 mil dry and allowed to cure for 15 days at ambient temperatures. Additional corrosion resistance can be achieved when the coated is applied with a higher film build.

  • 1 mil dry – Pass 250-300 hours
  • 2 mil dry – Pass 450 hours
  • 4 mils dry – Pass 600 hours
  • 6+ mils dry – Pass 750 hours
  • Exterior Exposure Test – Coating was applied to steel panel at 1 mil dry and allowed to cure for 15 days at ambient temperatures. Panel was positioned for southern exposure for an indefinite amount of time. After 24 months exposure, panel does not exhibit any blistering, cracking, spot rusting or delamination of film.

    Information provided by Blue River Coatings

    Available Properties
    • Specific Gravity
    • Density
    • Solids Content
    • Volatile Organic Compounds (VOC) Content
    • pH
    • Impact Test
    • Boiling Point
    • Flash Point
    • Dry Time
    • Shelf Life
    • Evporation rate
    • Pencil Hardness
    • Tape Adhesion
    • Theoretical Coverage
    • Vapor Density
    • Water Submersion
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。