Blue River Coatings High Performance Acrylic Sanding Sealer

 

Subcategory: Acrylic; Thermoset; Polymer

Material Notes:
BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is a waterbased wood sealer to fill the grain. The product is designed to be a sandable self-sealing topcoat for wood. HIGH PERFORMANCE ACRYLIC SANDING SEALER offers superb application properties, low foam, good adhesion, and excellent sanding properties. HIGH PERFORMANCE ACRYLIC SANDING SEALER dries quickly (eliminating excessive grain raise on wood) and provides excellent sealing properties to help repel water. The product is designed to work in conjunction with Blue River Coatings Wood Stains and Topcoats.

Enviromental Advantages:BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated, dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent grain filler
  • Minimal grain raising
  • Dry to touch in 15 minutes and Dry to sand in 30 minutes at 70°F and 50% humidity
  • Can be applied in a wide variety of temperature and humidity conditions
  • Water is used for clean-up
  • Non-Hazardous
  • Shelf life of 1 year
  • Non-Flammable
  • Uses

  • Any wood surface that can be sanded, stained, or selaed
  • Information provided by Blue River Coatings

    Available Properties
    • Specific Gravity
    • Density
    • Solids Content
    • Volatile Organic Compounds (VOC) Content
    • Boiling Point
    • Flash Point
    • Dry Time
    • Shelf Life
    • Flexibility
    • Pencil Hardness
    • Theoretical Coverage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。