MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Chevron 1000 THF

 

Subcategory: Fluid

Key Words: CPS Number: 226606; MSDS Number: 7648

Material Notes:
Features

Chevron 1000 THF (formerly Chevron Tractor Hydraulic Fluid and Amoco 1000 Fluid) is a high quality, multifunctional fluid, specially formulated for use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other equipment employing a common fluid reservoir.

It is formulated with ISOSYN™ base stocks, a viscosity index improver, oxidation and corrosion inhibitors, antiwear and film strength additives, an antifoaming agent, and a pour point depressant.

Its distinctive orange color allows for easy product identification and leak detection.

ApplicationsChevron 1000 THF is recommended for use as a mutifunctional fluid in all types of farm tractors an equipment. It can be used in any application which calls for the following OEM lubricant specifications:

  • AGCO-improved power fluid 821XL
  • John Deere-J20C
  • Ford New Holland-ESN-<2C134-D, FNHA 2 C 201
  • Massey Ferguson-M1135, M1141, M1143
  • White Farm Equipment-Q-1826
  • Case Corperation-JIC-143, JIC-145, MS 1206, MS 1207, MS 1209, MS 1210 (TCH)
  • Oliver-Type 55
  • Minneapolis-Moline-Fluids
  • Caterpillar-TO-2, MTO
  • Renk-Bus Automatic Transmission Fluid
  • Kubota-UDT
  • International Harvester-B6
  • VolvoWB 101

Available Properties
  • API Gravity
  • Brookfield Viscosity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。