Chevron Automatic Transmission Fluid MERCON® V

 

Subcategory: Fluid

Key Words: CPS Number: 226719; MSDS Number: 8061

Material Notes:
General Description

Beginning with the 1997 model year, Ford introduced a higher performance level ATF with the MERCON V specification. Many Ford automatic transmissions from 1999 on will require a MERCON V fluid. The most notable exceptions are the E40D, 4R100, and CD4E transmissions, which still specify regular MERCON ATF.

Chevron ATF MERCON® is fully approved for MERCON V, as well as DEXRON®-III and MERCON® approved. It provides excellent performance in frigid cold and is formulated to resist viscosity breakdown for long fluid life.

Applications

Chevron Automatic Transmission Fluid MERCON V is designed specifically for use in Ford Motor Compay transmissions that require a MERCON V fluid. The enhanced properties of the MERCON V specification offer premium performance in MERCON or DEXRON-III applications.

Available Properties
  • API Gravity
  • Brookfield Viscosity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。