Chevron Mchanism LPS® Hydraulic Oil, ISO 32

 

Subcategory: Fluid

Key Words: CPS Number: 255687; MSDS Number: 7580

Material Notes:
Features

Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor parts in heavy duty service.

Applications

Chevron Mechanism LPS Hydraulic Oils are high performance hydraulic oils recommended for use in all circulating oil systems providing power for hydraulics or hydraulic motors in heavy duty service.

Chevron Mechanism LPS hydraulic Oils have Vickers 35VQ25 vane pump approval and meet the requirements of:

  • DIN 51 524 (HVLP) gear test
  • FZG test load stage 10 (ISO 32, 46, 68)
which demonstrates outstanding pump protection under the most severe conditions.

Do not use in high pressure systems in te vicinity of flames, sparks and hot surfaces. Use only in well-ventilated areas keep container closed.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。