Chevron FM Synthetic Compressor Oil, ISO 46

 

Subcategory: Fluid

Key Words: CPS Number: 231019; MSDS Number: 7291

Material Notes:
Features

Chevron Synthetic Compressor Oil FM is a PAO based, synthetic, food grade, compressor oil.

Although Chevron Synthetic Compressor Oil FM offers a reduced risk of fires and explosions, it is not a fire-resistant fluid.

Applications

Chevron Synthetic Compressor Oil FM is recommended for both rotary and reciprocating air compressors. It is particularly useful in applications where incidental food contact may occur with oil in the discharge air.

Chevron Synthetic Compressor Oil FM may also be used where an R&O or mild antiwear hydraulic oil with high temperature stability and excellent low temperature fluidity performances are required.

Chevron Synthetic Compressor Oil FM is fully compatible in ammonia refrigerant systems as well as systems containing R 12 refrigerant. Chevron Synthetic Compressor Oil FM is not compatible with HFC-134A type refrigerant.

Chevron Synthetic Compressor Oil FM is similar to mineral oil in its compatibility with paints, seals, gaskets and hoses. Some examples of commonly used materials are1: Celcon®, Delrin®, epoxy paint, high nitrile Buna N, nylon, oil-resistant alkyd, PBT, Teflon®, and Viton®.

Available Properties
  • Specific Gravity
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Wear
  • Pour Point
  • Flammability Test
  • Flash Point
  • Demulsibility at 54°C, mL
  • Foaming Tendency Sequence I
  • Foaming Tendency Sequence II
  • Foaming Tendency Sequence III
  • Rust preventative Test Procedure B
  • Rust Procedure A, Distilled Water
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。