Chevron Quenching Oil 70

 

Subcategory: Fluid

Key Words: CPS Number: 233641; MSDS Number: 2582

Material Notes:
Features

Chevron Quenching Oil 70 is a premium quality quenching oil.

It is designed to provide controlled cooling of steel which is important in steel hardening. When quenching is started, Chevron Quenching Oil 70 provides a high initial cooling rate inducing maximum hardness, yet once the critical transformation temperature is passed, the ideal fluid cooling rate decreases to eliminate the possibility of stresses and metal distortion.

Applications

Chevron Quenching Oil 70 is recommended for use

  • when deep and uniform hardening is required in steels having small grain size or wide variation in grain size
  • in steels with lean alloy content
  • in parts having variable sections or odd shapes
  • in steels having variable hardenability
This highly stable oil resists the oxidizing effects of quenching and is less sensitive to the effects of agitation. It is highly heat resistant. No additive replacement is required and, in normal service, the product retains the original viscosity indefinitely. Because of its ability to adhere to smooth or shiny surfaces, Chevron Quenching Oil 70 is also recommended for use when parts must retain a bright finish.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flammability Test
  • Flash Point
  • Quenching Time, s
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。