Chevron Black Pearl® Grease EP, NLGI 1

 

Subcategory: Fluid; Lubricant

Key Words: CPS Number: 254592; MSDS Number: 7237

Material Notes:
Features

Chevron Black Pearl Greases EP are multipurpose, extreme pressure, water-resistant greases.

They are formulated with ISOSYN® base stock, a polyurea thickener, and rust and oxidation inhibitors. They are black in color and smooth and buttery in texture.

Applications

Chevron Black Pearl Greases EP provide outstanding film strength and adhesive properties. As a result, these products are particularly effective in providing superior wear protection in heavily loaded and shock load conditions.

Chevron Black Pearl Greases EP stay in place, sticking to bearing surfaces and, thus, provide excellent lubrication under a wide range of operating conditions. They perform particularly well in roller bearings. These products provide exceptional water wash out results. They perform well in applications where cascading water or actual bearing submergence can occur. The rust inhibitors effectively protect bearing surfaces against corrosion. Pumpability is excellent over a wide range of temperatures as indicated by the Lincoln ventmeter test and the relatively low pressure drop in piping. Oxidation inhibitors ensure long life in storage and in use. In addition, Chevron Black Pearl Greases EP also perform well at high temperatures.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Penetration
  • Penetration P(0), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Flash Point
  • Dropping Point
  • Bearing Rust
  • Color
  • Corrosion, Copper Strip Test 3h
  • Lincoln Ventmeter, psig at 30 s, at -22°F
  • Lincoln Ventmeter, psig at 30 s, at 0°F
  • Lincoln Ventmeter, psig at 30 s, at 30°F
  • Lincoln Ventmeter, psig at 30 s, at 75°F
  • Texture
  • Thickener, % / type
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。