Chevron Wheel End Grease,

 

Subcategory: Fluid; Lubricant

Key Words: CPS Number: 250605; MSDS Number: 7894

Material Notes:
Features

Chevron Wheel End Grease is a high performance grease specifically engineered for trailer wheel-ends operating in most conditions.

It is formulated with ISOSYN™ base stocks, a unique polyurea complex thickener that provides built-in extreme pressure performance, rust and oxidation inhibitors and a specially enhanced anti-oxidant package.

It is green in color with a smooth texture.

Applications

Trailer Lubrication - Chevron Wheel End Grease is recommended for use in trailer axles. It will lubricate at temperatures as low as -40°C (-40°F) and continues to lubricate efficiently at temperatures up to 160°C (320°F). It provides many advantages in trailer axle lubrication :

  • Good low temperature properties (starting torque)
  • Oxidation resistance at high temperatures
  • Low incidence of seal leakages through use of a grease, as compared with the conventional SAE 80W 90 gear oil
  • Excellent antiwear performance throughout the operating temperature range.

Industrial Lubrication - Chevron Wheel End Grease lubricates yearlong. Along with wide temperature range performance, Chevron Wheel End Grease provides excellent industrial equipment lubrication with a robust additive package that resists oxidation, protects against rust, enhances antiwear properties and ensures long lubricating life.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Wear
  • Penetration
  • Penetration P(0), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point
  • Bearing Rust
  • Color
  • Low Temperature Starting Torque, -40°F, Nm
  • Texture
  • Thickener, % / type
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。