Chevron Shingle Oil

 

Subcategory: Fluid

Key Words: CPS Number: 213304; MSDS Number: 4223

Material Notes:
Features

Chevron Shingle Oil is a straw colored, low viscosity oil designed for use as a shingle or shake dressing for shake roofs, wooden fencing, wood siding, and log homes.

Chevron Shingle Oil penetrates the wood surface to enhance or replace natural oils and resins leached out by cyclical exposure to sun and rain. Although Chevron Shingle Oil retards the aging process, it will not renew wood that is already weather damaged.

Applications

Loose dirt and debris should be removed before the oil is applied. The roof should be hosed with water 24 hours prior to application to lessen the possibility of over application. Alternatively, a licensed contractor can power wash the roof thereby removing weatherdamaged wood, allowing oil to absorb into new wood.

Chevron Shingle Oil may be applied by brushing or spraying. The typical application rate is 150-300 square feet per gallon. Application rate depends on the type of wood and the rate at which the oil saturates the wood.

Do not overapply — Over application may lead to shingle or shake "cupping" and the presence of oil in rainwater runoff.

Do not add color pigments — as they will lump and settle out.

Do not walk on treated surfaces — Chevron Shingle Oil is a petroleum oil and is slippery.

Do not use on flat surfaces, such as decks. Properly licensed contractors may add certain chemicals, such as antifungal agents and other substances, to Chevron Shingle Oil. Be sure to find out what safety or health restrictions may apply to these additives.

Available Properties
  • API Gravity
  • Volatile Organic Compounds (VOC) Content
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。