Conoco Soluble Oil ISO Grade 32

 

Subcategory: Fluid

Material Notes:
Description: Conoco Soluble Oil is a general-purpose oil suited for a wide variety of cutting and grinding operations that require a combination water-soluble lubricant and coolant. Soluble Oil is a carefully balanced blend of a high-quality mineral oil and emulsifying agents. The recommended mixing ratio is 5 vol. % soluble oil to 95 vol. % water. The typical operating range is 3 vol. % soluble oil/97 vol. % water to 10 vol. % soluble oil/90 vol. % water. However, at the lower range of 3 vol. %, the antirust characteristics of the mixture may be reduced. Two important maintenance items are vital for optimum Soluble Oil performance. First, maintain the correct oil-water ratio. Always add oil to water; never add water to oil. Water loss due to evaporation will enrich the emulsion, while filtration of used fluid will remove oil and dilute the emulsion. Second, institute a program to prevent the growth of odorcausing bacteria. This program should consist of regular treatment of the Soluble Oil system with a germicide and the periodic draining and cleaning of the system with a disinfectant solution, such as bleach. This maintenance program will bring maximum benefits from Soluble Oil.

Information provided by ConocoPhillips.

Available Properties
  • Density
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • ASTM Color
  • Emulsion Stability, 95% Water-5% Oil
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。