Conoco Bentone Grease NLGI No. 2

 

Subcategory: Fluid; Lubricant

Material Notes:
Description: Conoco Bentone Grease is a high-quality, smooth-textured, clay based grease developed for heavy-duty industrial machinery operating at very high temperatures. Unlike conventional soap-based greases, has excellent storage stability and retains its consistency at high temperature. In addition, it adheres to the surface to which it is applied and has excellent water washout characteristics. It is recommended for medium to large low-speed bearings commonly found in kilns, steel mills, aluminum, glass, rubber and cement plants where conventional soap-thickened greases normally fail due to the extreme high temperatures encountered. Frequent relubrication intervals are recommended under these conditions to minimize bearing failure due to lack of lubrication.

Information provided by ConocoPhillips.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Load Wear Index
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Penetration P(60), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Dropping Point
  • Color
  • Thickener
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。