Conoco Moly Poly Grease NLGI No. 2

 

Subcategory: Fluid; Lubricant; Organic Soap Gellant

Material Notes:
Description: Conoco Moly Poly Grease is a long-life, lithium 12-hydroxy grease for chassis, wheel bearings, ball joints, U-joints, tie-rod ends, steering knuckles and brake self-adjusting screws found in automobiles, trucks and farm and off-road equipment. Its polyethylene and molybdenum content reduces wear and noise. The combination of solid lubricants (moly and poly) with light viscosity base oil make this grease an excellent choice for high-speed antifriction bearings subject to shock loading and for use year round in most climates. Specifically designed as an excellent chassis grease for the transportation industry, Moly Poly Grease meets Ford ESA-MIC75-B and Mack MG-C specifications.

Information provided by ConocoPhillips.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Load Wear Index
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Penetration
  • Penetration P(60), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Dropping Point
  • ASTM Rust A&B
  • Color
  • Film Strength Durability
  • Film Strength Durability Scar Width
  • Molybdenum Disulfide
  • Oil Separation
  • Oxidation Stability
  • Penetration After Oxidation
  • Polyethylene
  • Soap Type (Thickener)
  • Stringiness Test
  • Timken Cup Corrosion Test
  • Water Washout
  • Wheel Bearing Leakage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。