MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Conoco SUPER-STA M NLGI No.0

 

Subcategory: Fluid; Lubricant; Organic Soap Gellant

Material Notes:
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C.V. joints, U-joints, and brake self-adjusting screws found in passenger cars, trucks, agricultural machinery and industrial equipment. They are also recommended for other applications that call for an EP lithium grease. Super-STA M Grease is composed of Super-STA Grease, with the addition of Molybdenum Disulfide (Moly). It meets Mack MG-C performance requirements for a chassis lubricant. Moly is used to reduce wear by maintaining lubrication under conditions of high friction and shock loads. Super-STA and Super-STA M Greases are manufactured with high viscosity-index paraffinic base oils thickened with lithium 12-hydroxy stearate soap stock. They contain rust and corrosion inhibitors, an effective EP additive and a tackiness agent. This additive combination results in quality greases which ensure excellent lubrication and longer bearing life.

Information provided by ConocoPhillips.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Load Wear Index
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Penetration P(60), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Dropping Point
  • ASTM Rust A&B
  • Color
  • Low Temperature Mobility
  • Roll Stability
  • Shear Stability
  • Soap Type (Thickener)
  • Wheel Bearing Leakage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。