Conoco ANDEROL® PQ ® AA-30 White Mineral Food Grade Oil, ISO Grade 68/100, SAE Grade 30

 

Subcategory: Fluid; Lubricant

Close Analogs: Anderol® is a registered trademark of The Anderol Company.

Material Notes:
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are recommended for use with hydraulic systems, vacuum pumps, compressors, bearings, gears, slides, ways and chains. It also can be used as a wipe down oil. PQ food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. PQ food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.”

Information provided by ConocoPhillips.

Available Properties
  • Specific Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • ASTM Color
  • Four Ball Wear
  • Falex Load Test
  • Timken Test
  • Pour Point
  • Flash Point
  • Copper Corrosion
  • Rust Test
  • Vickers Vane Pump Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。