Donnelly Bros APG # 2 Super Clean All Purpose Mold Grease

 

Subcategory: Fluid; Lubricant

Material Notes:
Clear, non-melting PTFE (Teflon type) extreme pressure All Purpose Grease (APG). Odorless, with a Vaseline-like texture. 100% waterproof. Mineral oil base.

APG is used in the automotive, appliance, electrical and medical industries. APG is being used in injection molding presses, molds (guide pins-slides & ejector pins), grinders, electric motors and RIM (resists isocyanate). Molders with very large presses use APG #1 (a thinner version of APG #2) to lubricate tie bars.

Because APG #2 stays in place and and does not melt, it is beneficial in lubricating mechanical parts of molds. APG does not migrate works well in constant metal temperature of 180° F to 200° F. (Note: The plastic molding material itself might be 500-600° F.) APG contains PTFE, which plates the metal with a one micron film thickness which reduces friction. The acceptance rate of APG for this use is high.

APG is approved by Ford, GM, and Chrysler Toxicology Departments. The USDA Food Grade approval is H2. (APG can be used in a food plant, but not where intimate contact is possible). All ingredients are USDA H1, except the thickener which is currently H2.

Information provided by Donnelly Bros. Inc.

Available Properties
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。