DURATHERM FG Paraffinic Heat Transfer Fluid

 

Material Notes:
Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contact (H1) and meets the requirements of 21CFR1783570.

Information provided by Duratherm.

Available Properties
  • Density
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Kinematic Viscosity at Elevated Temperature
  • Molecular Weight
  • Vapor Pressure
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  • Pour Point
  • Flammability Test
  • Flash Point
  • Distilation Range at 90%
  • Distiliation range at 10%
  • Max Bulk Temp (°F)
  • Max Film Temp (°F)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。