ExxonMobil Thermrex Series R-21

 

Subcategory: Fluid

Material Notes:
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and thermal stability, demulsibility, and nonferrous compatibility. The use of such ingredients results in quench oils that provide uniform steel hardness, long batch life, resistance to sludge formation, and minimum deformation. Thermrex D-10, R-21, and V-32 are mineral-oil blends carefully selected to approximate 100 SUS at 100°F. They yield consistent Relative Cooling Indices (RCI) of 95 to 160. Thermrex F-43 is a fast quench oil augmenting selected base stocks with additive technology to provide an RCI of 195. In addition, Thermrex R-21, V-32, F-43 are "gapped" to yield controlled distillation ranges from specific base stocks.

The Thermrex Series oils are excellent media for rapidly cooling alloy steels to achieve optimum strength and toughness. The selection of the particular grade of quench oil depends on the cooling rate desired to prevent cracking and distortion. Thermrex Series oils D-10, R-21, V-32, and F-43 are most effective with agitation at batch temperatures of less than 150°F.

Available Properties
  • Specific Gravity
  • Kinematic Viscosity at 40°C (104°F)
  • Pour Point
  • Flash Point
  • Cooling Rate, ASTM D6200, F/Sec
  • GM Quenchometer, %Quench Time, sec
  • GM Quenchometer, Relative Cooling Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。