ExxonMobil Mobil Jet Oil II

 

Subcategory: Fluid

Material Notes:
Mobil Jet Oil II is a high performance aircraft-type gas turbine lubricant formulated with a combination of a highly stable synthetic base fluid and a unique chemical additive package.  The combination provides outstanding thermal and oxidative stability to resist deterioration and deposit formation in both the liquid and vapour phases, as well as excellent resistance to foaming. The effective operating range of Mobil Jet Oil II is between -40ºC (-40 ºF) and 204 ºC (400ºF). Mobil Jet Oil II is engineered for aircraft gas turbine engines used in commercial and military service requiring MIL-PRF-23699 level performance.  It also is recommended for aircraft-type gas turbine engines in industrial or marine service applications.

Mobil Jet Oil II is recommended for aircraft gas turbine engines of the turbo-jet, turbo-fan, turbo-prop, and turbo-shaft (helicopter) types in commercial and military service.  It is also recommended for aircraft-type gas turbine engines used in industrial or marine applications. Mobil Jet Oil II is approved against U.S. Military Specification MIL-PRF-23699.  It is also compatible with other synthetic gas turbine lubricants meeting MIL-PRF-23699.  However, mixing with other products is not recommended because the blend would result in some loss of the performance characteristics of Mobil Jet Oil II. Mobil Jet Oil II is compatible with all metals used in gas turbine construction, as well as with F Rubber (Viton A), H Rubber (Buna N), and silicone seal materials.

Available Properties
  • Density
  • Viscosity Measurement
  • Viscosity Measure
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Evaporation Loss
  • Total Acid Number
  • Pour Point
  • Flammability Test
  • Flash Point
  • Foam Sequence I, ASTM D1130
  • Foam Sequence II, ASTM D893
  • Foam Sequence III, ASTM D893
  • Foam Stability, after 1 min settling, mL
  • Rubber Swell, %
  • Ryder Gear, Ave, lb/in % Hercolube A
  • Sonic Shear Stability, KV change %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。