ExxonMobil Exxon Hyjet V

 

Subcategory: Fluid

Material Notes:
Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability means extent of fluid degradation in aircraft systems will be less than Type IV fluids, in-service fluid life will be longer, and aircraft operator maintenance costs will be lower. HyJet V provides excellent high and low temperature flow properties (kinematic viscosities) and rust protection. HyJet V has also demonstrated an improvement over the erosion protection performance afforded by Type IV fluids.

Exxon HyJet V is designed for use in commercial aircraft phosphate ester hydraulic systems. It meets the SAE AS1241 requirements and is included in the Airbus NSA307110 and Boeing BMS 3-11M qualified products list. It is compatible in all proportions with commercial Type IV and Type V phosphate ester aviation hydraulic fluids.

Available Properties
  • Density
  • Specific Gravity
  • Viscosity Measurement
  • Viscosity Measure
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Evaporation Loss
  • Total Acid Number
  • Bulk Modulus
  • Electrical Resistivity
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Pour Point
  • Flammability Test
  • Flash Point
  • Foam Sequence I, ASTM D1136
  • Foam Sequence II, ASTM D893
  • Foam Sequence III, ASTM D893
  • Particle Count, NAS 1638 Class
  • Sonic Shear Stability, KV change %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。