ExxonMobil Exxon Hyjet IV-A

 

Subcategory: Fluid

Material Notes:
Exxon HyJet IV-Aplus is a fire-resistant phosphate ester hydraulic fluid designed for use in commercial aircraft. It is the best-performing Type IV fluid and offers to a great extent many of the performance capabilities of Type V fluids, including high temperature stability, low density, and rust protection. It is superior to all other Type IV fluids in these respects. Exxon HyJet IV-Aplus meets the specifications of all major aircraft manufacturers and SAE AS1241.

Exxon HyJet IV-Aplus fire-resistant aviation hydraulic fluid is used in commercial aircraft hydraulic systems where phosphate hydraulic fluids are recommended. Exxon HyJet IV-Aplus meets or exceeds the following industry and builder specifications.  It is approved against the aircraft manufacturer requirements and is included in their Qualified Products Lists.

Available Properties
  • Density
  • Specific Gravity
  • Viscosity Measurement
  • Viscosity Measure
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Evaporation Loss
  • Total Acid Number
  • Bulk Modulus
  • Electrical Resistivity
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Pour Point
  • Flammability Test
  • Flash Point
  • Foam Sequence I, ASTM D1137
  • Foam Sequence II, ASTM D893
  • Foam Sequence III, ASTM D893
  • Particle Count, NAS 1638 Class
  • Sonic Shear Stability, KV change %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。